highlandsflyer
Retro Wizard
- Feedback
- View
I have been looking inside my stays and I want to sort the rust out before I treat them.
I have used electrolysis in the past. I only want to do the stays (no rust on the 853 front triangle) so I will be hanging the frame over a tub with just the stays in, first the chain stays then the seat stays. I can't blast the inside after so am going to run pressurised water through to clear the detritus.
I haven't used it on gear where there was paint left, so it is presumably going to mess the paint up on the outside, but maybe I can add some nipples and run the electrolyte through the stays without bathing them?
Thoughts?
I have used electrolysis in the past. I only want to do the stays (no rust on the 853 front triangle) so I will be hanging the frame over a tub with just the stays in, first the chain stays then the seat stays. I can't blast the inside after so am going to run pressurised water through to clear the detritus.
I haven't used it on gear where there was paint left, so it is presumably going to mess the paint up on the outside, but maybe I can add some nipples and run the electrolyte through the stays without bathing them?
Thoughts?