Won't that melt the brazing
Laying continuous beads would run that risk but the way to do it would be like welding thin sheet. Short pulses of weld with a pause between each pulse to allow the dropout to cool. Not a great technique for sheet because it runs a risk of pin holes and cold joints but this is just to fill the gouges.
 